Home Facts industry

Anti-corrosive paint water weather

Anti-corrosive paint water weather

Write: Kasen [2011-05-20]
Scope
1 to the open steel equipment or materials, concrete corrosion protection can also be used in chemical equipment, oil equipment, power equipment, railways, bridges, pipelines, automobiles, tractors, cranes, boilers, machine tools, steel plants, wood, hydraulic facilities, municipal facilities, manufacturing and maintenance, especially for anti-corrosion primer coastal and humid areas.
Key Features
2.1 corrosion ability. By excellent corrosion resistance and weather resistant rubber compound compound of binder, so that the coating greatly increased corrosion resistance, can prevent the penetration of isolated corrosion medium.
2.2 excellent weather resistance. Alkali salt weathering performance of coatings is excellent, and has a strong acid, salt, alkali, water-resistance, bending properties.
2.3 easy to use. Single component, one into the film thickness, from space constraints, to adopt a common construction method, at room temperature can be cured film.
Construction Method
3.1 Mixing and dilution: the paint to the barrel end of a thorough mixing without sediment, if indeed too thick, can be added special paint thinner, the amount of 3 to 5%.
3.2 Surface treatment requirements: coating metal surface, sand blasting, shot blaster to reach the national standard Sa2. The class. Rust completed the necessary surface to clean, and clean the surface.
3.3 Coating thickness: High pressure airless spray, a gas spray, each about 95 m dry film thickness of about manual brush thickness of about 90 m.
3.4 Theory of consumption: if you do not consider the actual construction of the painting environment, coating method, coating technology, surface condition and structure, shape, surface area size of the general consumption of about 0.20kg / .
3.5 In order to coating formation, the best high pressure airless spray, airless spray, in the absence of high-pressure condition, only used a gas spray, hand brush painting method as the third choice.
3.6 Finally, after the completion of a paint coating to be cured naturally for 7 days to put to